dc.contributor.author | Aydin, Kemal | |
dc.contributor.author | Hidiroglu, Mehtap | |
dc.contributor.author | Kahraman, Nizamettin | |
dc.date.accessioned | 2023-01-27T05:50:28Z | |
dc.date.available | 2023-01-27T05:50:28Z | |
dc.date.issued | 2022 | en_US |
dc.identifier.citation | Transactions of the Indian Institute of MetalsVolume 75, Issue 5, Pages 1279 - 1291May 2022 | en_US |
dc.identifier.uri | https://link.springer.com/article/10.1007/s12666-021-02482-5 | |
dc.identifier.uri | https://hdl.handle.net/20.500.12440/5578 | |
dc.description.abstract | Automotive industry in recent years, has gained great importance. In line with this, DP600 and DP800 dual-phase steels and the electrical resistance spot welding method were used in the study. During the experimental trials, different welding currents (6, 7, and 8 kA) were selected and all other welding parameters were kept constant. The effects of the welding parameters on microstructure, hardness, tensile-shear, and cross-tensile strength were analyzed. In the phase measurements, 27.06–29.97% martensite and 70.73–73.85% ferrite phases were found. When the hardness values in the HAZ regions were examined, it was seen that the highest hardness values were 356 ± 5 HV in the DP600 and 451 ± 5 HV in the DP800 with a current intensity of 6 kA. Consequently, it was determined that tensile-shear and cross-tensile strengths had increased in parallel with the increase in the welding current and the highest values were determined as 8 kA–15.91 kN in tensile shear and 8 kA–4.91 kN in cross-tensile strength. © 2021, The Indian Institute of Metals - IIM. | en_US |
dc.language.iso | eng | en_US |
dc.publisher | Springer Nature | en_US |
dc.relation.ispartof | Transactions of the Indian Institute of Metals | en_US |
dc.rights | info:eu-repo/semantics/restrictedAccess | en_US |
dc.subject | DP600 | en_US |
dc.subject | Dual-phase steel | en_US |
dc.subject | Resistance spot welding | en_US |
dc.subject | DP800 | en_US |
dc.title | Characterization of the Welding Zone of Automotive Sheets of Different Thickness (DP600 and DP800) Joined by Resistance Spot Welding | en_US |
dc.type | article | en_US |
dc.relation.publicationcategory | Makale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı | en_US |
dc.department | Meslek Yüksekokulları, Gümüşhane Meslek Yüksekokulu, Elektronik ve Otomasyon Bölümü | en_US |
dc.authorid | 0000-0003-2951-4657 | en_US |
dc.identifier.volume | 75 | en_US |
dc.identifier.issue | 5 | en_US |
dc.identifier.startpage | 1279 | en_US |
dc.contributor.institutionauthor | Aydin, Kemal | |
dc.identifier.doi | 10.1007/s12666-021-02482-5 | en_US |
dc.identifier.endpage | 1291 | en_US |
dc.authorwosid | AHC-0404-2022 | en_US |
dc.authorscopusid | 54952090400 | en_US |