Comparison of Mechanical Properties Obtained for Armor Steels: Conventional Methods vs. Nanoindentation
(ASTM International, 2023)The mechanical properties of three armor steels, namely Ramor 500, Ramor 550, and Armox Advance, were acquired by nanoindentation and conventional methods, and then the results were compared. To this goal, samples were ...